Car window glass

Post by Jan de Jong »

Hello ! Please can anybody give me a schedule for firing and slumping a bowl of Car window Glass (I hope I use the right words in English for this material :) ) Thank you, Jan from Holland
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Car window glass

Post by DonMcClennen »

Car window glass use to be 2 thin layers of a glass sandwich with a thin plastic layer in the middle. If this is still the way its made then fusing is not an option..
"The Glassman"
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Car window glass

Post by Rick Wilton »

Car WINDOWS are tempered....... car windshields are laminated.

Windows good to fuse

Windshields NOPE
Rick Wilton
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Car window glass

Post by Jan de Jong »

Rick Wilton wrote:Car WINDOWS are tempered....... car windshields are laminated.

Windows good to fuse

Windshields NOPE
Thank you for your answer and sorry for the late response (waiting on a mail that there was a post, but that was in the paste !) But do you have a schedule for fusing and slumping this glass (or is that the same as "normal" window glass) ?? Jan de Jong (from Holland)