I've had what seems to be called rolled figure glass on a shelf for years. One side smoothish, the other patterned from a roller. Green, yellow and purple pieces. From windows and doors, it's beautiful glass. I'm thinking of slumping, light and easy, but unsure if the colour will hold. Has anyone experience or is it try a small bit and see. Thanks guys and gals.

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: coloured rolled figure glass

Postby Judd » Wed Aug 16, 2017 1:30 pm

This is stained glass window glass, not fusing glass?

If it's stained glass window glass, who knows? Many times they will strike to a Poop Color that NO ONE WILL BUY or WANT!!!

But, hey, experiment. Throw a small slice in the kiln when you do your next batch and see what happens.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 17 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com