Making a rainbow

Postby Jan de Jong » Fri Jun 30, 2017 2:57 pm

Hello ! Is there a simple way to make a "rainbow" (half-circle) with 6-7 colours ? Jan de Jong

jim simmons
Posts: 420
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Making a rainbow

Postby jim simmons » Fri Jun 30, 2017 3:58 pm

Sure.
cut a circle then cut it in half and layer different frits on it.
The other Jim

Jan de Jong
Posts: 78
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Making a rainbow

Postby Jan de Jong » Sun Jul 02, 2017 4:47 am

jim simmons wrote:Sure.
cut a circle then cut it in half and layer different frits on it.
The other Jim
Thank you Jim ! Is there a way to do it with sheet glass (as I still did not work with frits and not have them). Is it possible with a saw ? Jan

Fiona Collins
Posts: 30
Joined: Sun Nov 17, 2013 9:10 am

Re: Making a rainbow

Postby Fiona Collins » Sun Jul 02, 2017 7:29 am

Cut a half sheet of clear and butt against 1/2 sheet of first colour. Place your circle cutter in the middle of the join, score half circle on the colour sheet, adust length in 15mm, leave base as is, run second score. Replace colour sheet with second colour, score with same setting as previous, adjust length in 15mm ... rinse and repeat 4 times. Carefully run and break out each segment

Jan de Jong
Posts: 78
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Making a rainbow

Postby Jan de Jong » Wed Jul 05, 2017 5:00 am

@ Fiona Collins: Thank you ! Jan


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 5 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron