I know this has probably been covered, but I can't find it. :oops:
I have a bowl that slumped way off center and I would like to flatten it.
Should I go with the opening up or down?
Thanks in advance
The other Jim
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: cooking in the kiln

Post by Sharol »

Hi Jim,

A few years ago, I flattened a 16" bowl to correct a flaw. I did it with the opening down towards the shelf. I slumped it super slow (could dig up the schedule if you're interested) and I was surprised at how well it turned out. It ended up being a flat, almost perfectly round blank, that I cold worked and eslumped into a bowl again. I think the width of the bowl contributed a lot to the success. I'm not sure something smaller would have worked as well.

Sharol