Tack fusing, but different
Hello, I did a full fuse with 2 layers Spectrum glass. After that full fuse I did a tack fuse with 2 layers on the first glass. Temp. 750 degrees Celsius. But the 2 layers had spread out, it look like a full fuse. Do you have to use a lower temp. by 4 layers ? Jan de Jong
-
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Tack fusing, but different
Sorry, perhaps placed in the wrong topic. Jan
Re: Tack fusing, but different
No, posting here is fine.
How long did you hold at 750?
How long did you hold at 750?
-
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Tack fusing, but different
For 10 minutes. JanJudd wrote:No, posting here is fine.
How long did you hold at 750?
Re: Tack fusing, but different
Are you sure your thermocouple is reading correctly?
Whatever the case, maybe hit your target temp for only 5 minutes?
Whatever the case, maybe hit your target temp for only 5 minutes?