Postby jim simmons » Tue Feb 27, 2018 6:13 pm

Can I cut a mullite kiln shelf with a skill saw without ruining the saw blade?
The other Jim

Kevin Midgley
Posts: 633
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: cutting a mulite kiln shelf with a skill saw

Postby Kevin Midgley » Tue Feb 27, 2018 9:08 pm

wet shelf diamond blade

DonMcClennen
Posts: 345
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: cutting a mulite kiln shelf with a skill saw

Postby DonMcClennen » Sat Mar 03, 2018 12:36 pm

Use a blade made for concrete or ceramics.
"The Glassman"


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com