Potmelt from transparent glass

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Potmelt from transparent glass

Post by Jan de Jong »

Hello ! Is it possible to do a potmelt with only transparant glass colours ? I did try it once.....all colours became dark ? Thank you ! Jan
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Potmelt from transparent glass

Post by DonMcClennen »

You will need to have your pot filled with at least 50% clear plus stick with lighter shades of transparent glass!
"The Glassman"
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Potmelt from transparent glass

Post by JestersBaubles »

Avoid reds, and pay attention to not mix reactive colors (or at least separate them from each other with a layer of clear).

Dana
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Potmelt from transparent glass

Post by Jan de Jong »

Thank you both for your answer ! I will try again. Jan de Jong
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Potmelt from transparent glass

Post by Sharol »

In addition to reds...orange and yellow transparents will have a tendency to opalize at pot melt temperatures. So, unless you’d like this effect, you should avoid these colors.

Sharol
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Potmelt from transparent glass

Post by Jan de Jong »

Thank you Sharol ! Jan