Page 1 of 1
Potmelt from transparent glass
Posted: Sat Aug 25, 2018 6:11 am
by Jan de Jong
Hello ! Is it possible to do a potmelt with only transparant glass colours ? I did try it once.....all colours became dark ? Thank you ! Jan
Re: Potmelt from transparent glass
Posted: Sun Aug 26, 2018 4:21 pm
by DonMcClennen
You will need to have your pot filled with at least 50% clear plus stick with lighter shades of transparent glass!
Re: Potmelt from transparent glass
Posted: Thu Aug 30, 2018 9:54 pm
by JestersBaubles
Avoid reds, and pay attention to not mix reactive colors (or at least separate them from each other with a layer of clear).
Dana
Re: Potmelt from transparent glass
Posted: Mon Sep 03, 2018 8:00 am
by Jan de Jong
Thank you both for your answer ! I will try again. Jan de Jong
Re: Potmelt from transparent glass
Posted: Fri Sep 07, 2018 10:57 pm
by Sharol
In addition to reds...orange and yellow transparents will have a tendency to opalize at pot melt temperatures. So, unless you’d like this effect, you should avoid these colors.
Sharol
Re: Potmelt from transparent glass
Posted: Sat Sep 15, 2018 4:56 am
by Jan de Jong
Thank you Sharol ! Jan