Postby ilkaplan » Sun May 12, 2019 8:02 pm

I just got a new Skutt Kiln, with new shelf, and kiln wash powder. My first two firings had lots of adherence to the glass (four of wash applied), but I am noticing that the wash that stays on the shelf is looking more paint-like and firm. The first application was pretty dusty even after firing and drying.
Does the wash adhere better after multiple full fuse firings?
Is the Skutt kiln wash not ideal?

Kevin Midgley
Posts: 720
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Do I need to “season” my new shelf?

Postby Kevin Midgley » Sun May 12, 2019 8:46 pm

Heat shelf.
Turn off power.
brush on kiln wash.
Yes it will sizzle.
Repeat until you cannot see shelf surface.
Helps to apply at right angles to previous coating.
Different kiln washes have different amounts of clay that cause it to stick or not stick to shelf.
Some people swear by Primo.
Bullseye's is good.

Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Do I need to “season” my new shelf?

Postby Ed Cantarella » Tue May 14, 2019 10:21 am

ilkaplan wrote:I just got a new Skutt Kiln, with new shelf, and kiln wash powder. My first two firings had lots of adherence to the glass (four of wash applied), but I am noticing that the wash that stays on the shelf is looking more paint-like and firm. The first application was pretty dusty even after firing and drying.
Does the wash adhere better after multiple full fuse firings?
Is the Skutt kiln wash not ideal?

Some folks (self) give the shelf a light rubbing(please use ventilation, dust is bad) with a cloth or dry paper towel (panyhose are great but my wife doesn't wear them :o ) after first firing with the 4 layers to smooth out any brush pattern, then give another light coat. Then just periodically. Same with molds. If you see scabbing of kiln wash after a fire it's time to wash off and start fresh - it's only gonna get worse and it's hard to smooth over a scab with wash.
*I'm a Primo man but BE is good too - have used both, small subtle differences.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

ilkaplan
Posts: 2
Joined: Sat May 04, 2019 1:04 pm

Re: Do I need to “season” my new shelf?

Postby ilkaplan » Fri May 24, 2019 2:29 pm

Thanks. Wash seems more solid with”hot”application technique.

Don Burt
Posts: 543
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: Do I need to “season” my new shelf?

Postby Don Burt » Sun May 26, 2019 8:51 am

I only recently learned to apply the primer to a hot shelf. My practice now is with a very warm shelf.....with the kiln at about 120F or so. I was surprised and pleased to see the result of using BE primer at their recommended mix ration: 5 to 1 water to powder. I was making it more thick and it was flaky after a short usage. With a warm shelf you can get a lot of coats on of really thin mixture in a short amount of time.

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Do I need to “season” my new shelf?

Postby Judd » Fri Aug 16, 2019 12:28 pm

I season my shelves all the time. I start off with a little olive oil and garlic, then add rosemary for that sharp flavor...

Joyce Walters
Posts: 80
Joined: Thu Nov 08, 2007 12:06 am
Location: Stevensville MT

Re: Do I need to “season” my new shelf?

Postby Joyce Walters » Sun Aug 18, 2019 4:43 pm

Funny funny man. Took me the briefest minute to laugh aloud.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 17 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron