Postby jim simmons » Mon Sep 02, 2019 6:39 pm

Do you need to apply ridigizer to fiberboard?
If so, how to apply.
Thanks in advance
the other Jim

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: ridigizer with fiberboard

Postby Kevin Midgley » Wed Sep 04, 2019 11:31 am

Rigidizer is great but I've found it attracts glass like flypaper attracts flies.
Question to ask is will it make the mold any better in some way that is worth that risk.

jim simmons
Posts: 463
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: ridigizer with fiberboard

Postby jim simmons » Wed Sep 04, 2019 3:34 pm

OK, thanks Kevin
I will try the fiberboard.
Will I need to apply a glass separator?

The other Jim.

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: ridigizer with fiberboard

Postby Kevin Midgley » Thu Sep 05, 2019 11:12 am

Oh I'd expect you to have to apply a separator otherwise I think you'd have heard of "this perfect mold material that never sticks to glass and you can use a zillion times" :lol: We'd have those specialist separator companies worried.
Everyone's kilns are different and the sources of mold materials vary by country and supplier.
I noted decades ago one particular material I could get in Canada was vastly superior to that which you had in the US but times and suppliers change so I don't know what the current situation is.
You always have to experiment and don't expect the first try to work the way you want it to.
Note I did not ever say not to use rigidizer I only warned about the rigidizer I could get here in Canada attracting glass like flies to flypaper.
What rigidizer does do is make the mold material more brittle for handling but that is my experience. What previously could be a dent can instead be a break of a mold if you are careless.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: ridigizer with fiberboard

Postby Bert Weiss » Thu Sep 05, 2019 8:22 pm

There are 2 kinds of rigidizer, colloidal silica and colloidal alumina. Silica tends to land on the surface and sticks to glass (often the pink stuff). Alumina is probably what the boards are made with in the first place (green stuff as I’ve seen it). I sinks in and doesn’t stick to glass as much. Boards come as LD MD or HD, light medium or heavy density.

Silica dies if it freezes so it isn’t shipped in winter. Alumina comes as a power you mix with water.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 9 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com