Postby Mike Garvey » Thu Mar 19, 2020 12:36 pm

I am thinking to add a small stainless washer to a kiln element (Kanthal) tail as it passes out of the kiln in order to prevent the tail from cutting into the soft firebrick. Can I use stainless or do I have to go the ceramic route? Thanks....Mike

Marty
Posts: 852
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Kiln element compatibility with stainless?

Postby Marty » Thu Mar 19, 2020 8:19 pm

Either will work. I used ss fender washers.

Kevin Midgley
Posts: 709
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Kiln element compatibility with stainless?

Postby Kevin Midgley » Thu Mar 19, 2020 10:11 pm

Ceramic tubes are available. Old knob and tube wiring tubes could work as well. Get your wiring inspected before using.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 10 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com