Combing with Reactives

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Combing with Reactives

Post by Sharol »

I'm revisiting combing, this time exploring how reactive glass behaves at higher temperatures. Both sides were combed and then sandblasted before slumping. This piece is 15.5" in diameter and about 3" deep. I apologize for the photos not being of better quality, but my photo gear is packed up at the moment, so I snapped these on the fly.

Sharol
Attachments
image.jpg
image.jpg
Joyce Walters
Posts: 80
Joined: Thu Nov 08, 2007 12:06 am
Location: Stevensville MT

Re: Combing with Reactives

Post by Joyce Walters »

Wow!
I really, really like this bowl.
Can you tell us what glasses you used in the reaction, and how high the temperature?
Thank you for sharing.
Joyce
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Combing with Reactives

Post by Morganica »

I very much like this, especially the drips. French Vanilla and, uhm...Turquoise Blue?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: Combing with Reactives

Post by Warren Weiss »

Sharol,
Beautiful !!
Warren
Last edited by Warren Weiss on Wed Sep 03, 2014 9:20 pm, edited 1 time in total.
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Post by Sharol »

Thank you!

I used Lt Cyan, French Vanilla and Dense White. The crackle and strip construction are Dense White. Both combings were done at 1675 degrees, about 30 degrees hotter than I usually go. It was interesting to see how the reactions in different portions of the composition intensified (or not!) with each firing.

Sharol
Jeanice
Posts: 35
Joined: Sun Jan 01, 2012 1:24 pm
Location: Wyoming, USA

Re: Combing with Reactives

Post by Jeanice »

Absolutely stunning Sharol! I would have a hard time parting with that one.
Jeanice
Drewcilla
Posts: 60
Joined: Fri Apr 11, 2008 9:10 am

Re: Combing with Reactives

Post by Drewcilla »

Ditto what Jeanice said. Simply beautiful.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Combing with Reactives

Post by Havi »

You always surprise me with wonderful pieces, Sharol!
I can't say 'God bless your hands" I think they are blessed already!!!

wonderful,
Thanks for sharing


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Post by Sharol »

My goodness, Havi! What a lovely thing to say. You warm the cockles of my soul :) Thank you!

Sharol
Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Re: Combing with Reactives

Post by Terry Ow-Wing »

exquisite =D> =D> =D>
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Combing with Reactives

Post by Buttercup »

I agree with everything that's been said. Gorgeous! Congratulations! Jen
Pat K.
Posts: 53
Joined: Thu Aug 04, 2005 12:33 pm
Location: Pittsburgh, PA

Re: Combing with Reactives

Post by Pat K. »

Just beautiful, Sharol, as always.
Patty

It often shows a command of language to say nothing - author unkown.
Haydo
Posts: 292
Joined: Fri Mar 14, 2003 9:55 am
Location: Eimeo, Qld., Australia
Contact:

Re: Combing with Reactives

Post by Haydo »

Have come back to this over the last few days, thinking whether or not say anything. Congratulations, it's a very thoughtful, well executed piece. Could easily get lost just looking into it. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Post by Sharol »

Thanks everyone for the encouraging comments! You stir up my energy!

Sharol
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Combing with Reactives

Post by twin vision glass »

Glorious, have you worked with the Reactive Ice and Reactive Cloud. I am glad the dense white took the high temperature. Leslie
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Post by Sharol »

Thank you, Leslie. Yes, I've worked with both in my combings. I particularly like the reactive Cloud, as the reaction seems to be more consistent than the Reactive Ice. Actually, I'm laying a piece up now that will incorporate both along with Lt Aquamarine. Hopefully it will go well and become part of a series.
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Combing with Reactives

Post by twin vision glass »

Can hardly waite for the results. Wonderful work . Les
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: Combing with Reactives

Post by KaCe »

What does your combing tool look like? Is it a comb? Or do you use a single tine? I am curious, as I've wanted to try this on some pieces that I didn't like as they are, and thought with some heat and a comb, I could alter it enough to enjoy it. Does it have a long handle? I guess I'm very curious... but grateful for any answers. I do love you design sense and your pallet... very nicely done. =D>
Sharol
Posts: 123
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Post by Sharol »

KaCe -

Here's a photo of my primary raking/combing tool. As you can see it has just one tip. It's about 34.5" from stem to stern and is made from stainless steel rod and tube.

Sharol
Attachments
Rake.JPG
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Combing with Reactives

Post by charlie »

just remember: unless you have a shutoff switch on the door/lid, part of the comb handle should be wood. this would be pretty dangerous if you didn't have a shutoff switch if you accidentally hit an element.

wood also doesn't conduct heat very well.
Post Reply