Another pic posting test

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Another pic posting test

Post by Steve Immerman »

Just testing how to post images:

Image

Steve

http://www.clearwaterglass.com
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

:arrow: Looks like it's working Steve. :mrgreen:

Ron :roll:
Kathie Karancz
Posts: 137
Joined: Wed Mar 12, 2003 3:49 pm
Location: Calgary, Alberta, Canada
Contact:

Post by Kathie Karancz »

Steve: Absolutely loved your plate. I just happened to have picked up 2 sheets of Adventurine Green on Saturday and now I'm pumped!!! Awesome..... :D
Kathie Karancz
Tribal Turtle
Victoria, British Columbia
http://www.tribalturtle.com
Carole Burton
Posts: 38
Joined: Mon Mar 10, 2003 12:57 pm
Location: Charleston, S.C.

Post by Carole Burton »

Steve. Love the way you handled the design elements. Looking good.

Also like the way you can roll the website site and see all the work without clicking back and forth. Makes viewing more enjoyable.

Carole...S>C> =D> =D> =D>
Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Post by Steve Immerman »

Thanks guys. Adventurine green is definitely fun to work with.

And, Kathie, I'm glad you like how the web site is arranged. It just keeps growing and growing...

Steve
slats
Posts: 110
Joined: Thu Sep 04, 2003 9:19 pm

sushi plates

Post by slats »

a beaut!.....may I ask what glue do you use for the cylinder legs....I have tried many kinds and they keep coming off.....Also, do you layer transparant glass on each other to develop different hues? Really sleek and chic!
Cher
Posts: 91
Joined: Tue Oct 07, 2003 8:59 pm
Location: MI
Contact:

inspiring

Post by Cher »

Honestly, so inspiring, I've had dreams about it!

Yo
>^..^<
Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Post by Steve Immerman »

Wow. Thanks for dreaming about it. I was up half the night thinking about my next piece...


The cylinder legs are pyrex rods, cut to length and polished as taught in Brock and Avery's class.

Seteve
slats
Posts: 110
Joined: Thu Sep 04, 2003 9:19 pm

glue

Post by slats »

what glue do u use?
Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Re: glue

Post by Steve Immerman »

doctac wrote:what glue do u use?
GE Silicone 2
Post Reply