This is a blue wine bottle flatten then fired with Paradise premixed white paint. I fired it to 1400 with a 10 min soak there is really no color lost from my before and after shots. Painting was inspired from a coin.
Image
Tom
Head Fool @ Tom's Foolery
http://www.picturetrail.com/tomsfoolery
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Post by Bert Weiss »

Nice work Tom.

I wonder how it would look if you did the paint and slump in one shot.