New Green Mica Bowl with Dichro Beads

Postby Michael McNerney » Mon Dec 22, 2003 9:44 am

New Green Mica Bowl with Dichro Beads

http://groups.msn.com/McNerneyGlassAblb ... &PhotoID=6

Any and all comments welcome

Thanks
Michael

twinkler2
Posts: 45
Joined: Fri Aug 22, 2003 2:37 pm
Location: Happy Valley, PA
Contact:

Postby twinkler2 » Mon Dec 22, 2003 12:34 pm

Very cool :)

I like your work

Me Kim

DonMcClennen
Posts: 368
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Postby DonMcClennen » Mon Dec 22, 2003 12:42 pm

Nice work! Clean design, clever use of this medium. Keep up the Excellent work.
Don
"The Glassman"

starchimes (Andrea)
Posts: 26
Joined: Tue May 20, 2003 11:39 am
Location: Dallas, TX
Contact:

Postby starchimes (Andrea) » Mon Dec 22, 2003 4:40 pm

Stunning bowl. Where are you guys getting the colored mica? I have found it in silver, copper and gold.

Michael McNerney
Posts: 41
Joined: Tue Mar 18, 2003 12:22 pm
Location: Hilliard, Ohio

Postby Michael McNerney » Mon Dec 22, 2003 5:25 pm

I get them at prizm art supplies in columbus ohio.
They are better known as Pearl-EX Pigments

Bonita (Nita) Crawford
Posts: 62
Joined: Mon Mar 10, 2003 11:17 pm
Location: Montgomery, AL

Postby Bonita (Nita) Crawford » Tue Dec 30, 2003 4:40 am

Michael, what a terrific bowl! Did you spray on the mica and cap the
entire blank with clear glass? Love your clean and flowing design.

Nita

Michael McNerney
Posts: 41
Joined: Tue Mar 18, 2003 12:22 pm
Location: Hilliard, Ohio

Postby Michael McNerney » Tue Dec 30, 2003 12:02 pm

Nita,
I fused the clear and black together first, then applied mica's. Capping micas can be kind of tricky, if ther kiln is to hot they sink and disapear, to cool and they can create air bubbles in you cap. So I say why risk it, put them on top and tell your buyer not to eat off of it. Some things are ment for decorative use only.
I hope that answers your question.

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Postby Tony Smith » Tue Dec 30, 2003 12:05 pm

Michael McNerney wrote:Nita,
I fused the clear and black together first, then applied mica's. Capping micas can be kind of tricky, if ther kiln is to hot they sink and disapear, to cool and they can create air bubbles in you cap. So I say why risk it, put them on top and tell your buyer not to eat off of it. Some things are ment for decorative use only.
I hope that answers your question.


Not that I condone or recommend eating off a piece of artwork, but why wouldn't you eat off it? The micas are inert and very rugged.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

Michael McNerney
Posts: 41
Joined: Tue Mar 18, 2003 12:22 pm
Location: Hilliard, Ohio

UPDATE:

Postby Michael McNerney » Tue Dec 30, 2003 12:05 pm

Thank you all for your interest and insight

UPDATE:This piece sold two weeks ago.

Michael

Michael McNerney
Posts: 41
Joined: Tue Mar 18, 2003 12:22 pm
Location: Hilliard, Ohio

Postby Michael McNerney » Tue Dec 30, 2003 12:11 pm

Tony,
I was under the impression that there would be a chance of ingesting
the micas. I didnt want to poison my client base, but if there is little or no risk of ingestion put some pasta in them and have a party.


Thanks for the info Toney

Bonita (Nita) Crawford
Posts: 62
Joined: Mon Mar 10, 2003 11:17 pm
Location: Montgomery, AL

Hooray on the sale of your wonderful bowl, Michael

Postby Bonita (Nita) Crawford » Tue Dec 30, 2003 3:50 pm

I wouldn't be surprised if the first person who saw it bought it!!

Nita


Post Reply

Return to “Photos and Stuff”

Who is online

Users browsing this forum: No registered users and 13 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron