Postby Susanbuckler » Sun Mar 17, 2013 8:24 am

I'm a newbie and this is my first photo posted. It's a 7" glass mosaic bowl. I learned to make glass mosaic fused bowls at Oakta Glass Studio in Batavia, NY. .....a great place to learn fusing skills. The bottomless mold used is one of Laurie Spray's molds, which as it has no bottom, sits flat.....great for someone with limited cold working equipment. If anyone reading this is from the Hudson Valley of NY, I'd like to make a connection. Thanks.
Attachments
image.jpg
Susan Buckler
Woodstock, NY

Susanbuckler
Posts: 68
Joined: Tue Aug 18, 2009 10:31 pm

Re: Glass mosaic bowl

Postby Susanbuckler » Sun Mar 17, 2013 8:27 am

Oops... I see the bowl is upside down....my apologies.
Susan Buckler
Woodstock, NY

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: Glass mosaic bowl

Postby Laurie Spray » Sun Mar 17, 2013 3:23 pm

Nice colors! Glad you like the molds!
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com

Mike Jordan
Posts: 94
Joined: Mon Nov 06, 2006 11:13 pm
Location: Hillsboro, OR
Contact:

Re: Glass mosaic bowl

Postby Mike Jordan » Sun Mar 17, 2013 9:23 pm

Nice job. It also looks like it would make a very nice lamp shade as well. :D

Mike
It's said that inside each of us is an artist trying to get out. Well mine got out... and I haven't seen him since.

Don Burt
Posts: 536
Joined: Sun Mar 09, 2003 8:45 pm
Location: Cincinnati, Ohio
Contact:

Re: Glass mosaic bowl

Postby Don Burt » Tue Mar 19, 2013 9:26 am

I like the design. Is the lighter blue glass opaque and the other colors transparent? Trying to understand the color cast in the shadow, and if the lighter blue is transparent, what color glass it must be to effect that result when plated over that amber color.

Raphael Schnepf
Posts: 24
Joined: Sat Oct 14, 2006 11:31 pm
Location: Milwaukie Oregon
Contact:

Re: Glass mosaic bowl

Postby Raphael Schnepf » Tue Mar 19, 2013 2:10 pm

Wondered how you stuck it to the ceiling.

JestersBaubles
Posts: 691
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Glass mosaic bowl

Postby JestersBaubles » Tue Mar 19, 2013 8:11 pm

The lighter blue looks transparent -- if you look at the closeup image, you can see bubbles.

My guess is the amber is frit to fill in the spaces between the blue glass.

Dana W.

Susanbuckler
Posts: 68
Joined: Tue Aug 18, 2009 10:31 pm

Re: Glass mosaic bowl

Postby Susanbuckler » Sat Mar 23, 2013 5:30 am

I use bullseye glass. Not sure what color the lighter blue is because it was unlabeled scrap glass. The dark blue is deep royal blue, the green is adventurine green and the frit is fine marigold yellow. It was made with a base of two layers of 90 clear. Thanks for the comments. This was the first time I used the morton board to make traiangles. Fun!
Susan Buckler
Woodstock, NY

Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Re: Glass mosaic bowl

Postby Dolores » Sun Mar 24, 2013 1:35 pm

Nice. Flip it over and it would make a gorgeous ceiling lamp :)

DOLORES


Post Reply

Return to “Photos and Stuff”

Who is online

Users browsing this forum: No registered users and 7 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com