Drop Ring Vessel - WarmGlass.com

Drop Ring Vessel

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
StaceyG
Posts: 40
Joined: Sun Feb 22, 2004 8:17 pm
Location: Baltimore, Maryland

Drop Ring Vessel

Postby StaceyG » Wed May 22, 2013 11:29 am

After much trial and error, I have a presentable drop ring vessel. I used 4 layers of glass, and it dropped about 5". 3 layers was sometimes just a little too thin. I like the feel of the heavier vessel with 4 layers, so I think I will stick with that. The colors remind me of the beach, so I am really happy with how it all turned out.
Attachments
292989_4985746848518_1670455770_n.jpg

Eryc F.
Posts: 50
Joined: Sun Apr 28, 2013 8:29 am
Location: Canton, MA
Contact:

Re: Drop Ring Vessel

Postby Eryc F. » Wed May 22, 2013 11:53 am

That's really nice! And elegant!

Tracy Fries
Posts: 41
Joined: Thu Jun 14, 2012 7:14 pm

Re: Drop Ring Vessel

Postby Tracy Fries » Wed May 22, 2013 1:24 pm

Lovely piece! Thank you for sharing.

la suisse
Posts: 26
Joined: Wed Jul 15, 2009 8:41 am

Re: Drop Ring Vessel

Postby la suisse » Wed May 22, 2013 2:33 pm

This is beautiful and I really do love the colors!

Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: Drop Ring Vessel

Postby Warren Weiss » Wed May 22, 2013 4:21 pm

Stacey,
Lovely work. What was the diameter of the hole in your drop ring? Thanks.
Warren

AndyT
Posts: 150
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Drop Ring Vessel

Postby AndyT » Wed May 22, 2013 5:57 pm

Way nice!

StaceyG
Posts: 40
Joined: Sun Feb 22, 2004 8:17 pm
Location: Baltimore, Maryland

Re: Drop Ring Vessel

Postby StaceyG » Wed May 22, 2013 7:52 pm

The hole in the center is about 3".

Havi
Posts: 589
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Drop Ring Vessel

Postby Havi » Thu May 23, 2013 1:49 am

StaceyG wrote:The hole in the center is about 3".



And how tall is it.
A nice piece, I like it.
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

StaceyG
Posts: 40
Joined: Sun Feb 22, 2004 8:17 pm
Location: Baltimore, Maryland

Re: Drop Ring Vessel

Postby StaceyG » Thu May 23, 2013 5:16 am

Its about 5" high.

Drewcilla
Posts: 60
Joined: Fri Apr 11, 2008 9:10 am

Re: Drop Ring Vessel

Postby Drewcilla » Fri May 24, 2013 10:42 am

Lovely. Thanks for sharing.


Post Reply

Return to “Photos and Stuff”

Who is online

Users browsing this forum: No registered users and 5 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com