Postby Sharol » Wed Sep 03, 2014 6:10 pm

I'm revisiting combing, this time exploring how reactive glass behaves at higher temperatures. Both sides were combed and then sandblasted before slumping. This piece is 15.5" in diameter and about 3" deep. I apologize for the photos not being of better quality, but my photo gear is packed up at the moment, so I snapped these on the fly.

Sharol
Attachments
image.jpg
image.jpg

Joyce Walters
Posts: 74
Joined: Thu Nov 08, 2007 12:06 am
Location: Stevensville MT

Re: Combing with Reactives

Postby Joyce Walters » Wed Sep 03, 2014 6:23 pm

Wow!
I really, really like this bowl.
Can you tell us what glasses you used in the reaction, and how high the temperature?
Thank you for sharing.
Joyce

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Combing with Reactives

Postby Morganica » Wed Sep 03, 2014 6:28 pm

I very much like this, especially the drips. French Vanilla and, uhm...Turquoise Blue?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: Combing with Reactives

Postby Warren Weiss » Wed Sep 03, 2014 8:56 pm

Sharol,
Beautiful !!
Warren
Last edited by Warren Weiss on Wed Sep 03, 2014 9:20 pm, edited 1 time in total.

Sharol
Posts: 111
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Postby Sharol » Wed Sep 03, 2014 9:08 pm

Thank you!

I used Lt Cyan, French Vanilla and Dense White. The crackle and strip construction are Dense White. Both combings were done at 1675 degrees, about 30 degrees hotter than I usually go. It was interesting to see how the reactions in different portions of the composition intensified (or not!) with each firing.

Sharol

Jeanice
Posts: 35
Joined: Sun Jan 01, 2012 1:24 pm
Location: Wyoming, USA

Re: Combing with Reactives

Postby Jeanice » Thu Sep 04, 2014 9:35 am

Absolutely stunning Sharol! I would have a hard time parting with that one.
Jeanice

Drewcilla
Posts: 60
Joined: Fri Apr 11, 2008 9:10 am

Re: Combing with Reactives

Postby Drewcilla » Thu Sep 04, 2014 1:01 pm

Ditto what Jeanice said. Simply beautiful.

Havi
Posts: 567
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Combing with Reactives

Postby Havi » Thu Sep 04, 2014 5:10 pm

You always surprise me with wonderful pieces, Sharol!
I can't say 'God bless your hands" I think they are blessed already!!!

wonderful,
Thanks for sharing


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

Sharol
Posts: 111
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Postby Sharol » Thu Sep 04, 2014 10:07 pm

My goodness, Havi! What a lovely thing to say. You warm the cockles of my soul :) Thank you!

Sharol

Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Re: Combing with Reactives

Postby Terry Ow-Wing » Sat Sep 06, 2014 1:54 am

exquisite =D> =D> =D>
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image

Buttercup
Posts: 544
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Combing with Reactives

Postby Buttercup » Sun Sep 07, 2014 6:43 pm

I agree with everything that's been said. Gorgeous! Congratulations! Jen

Pat K.
Posts: 53
Joined: Thu Aug 04, 2005 12:33 pm
Location: Pittsburgh, PA

Re: Combing with Reactives

Postby Pat K. » Sun Sep 14, 2014 10:14 am

Just beautiful, Sharol, as always.
Patty

It often shows a command of language to say nothing - author unkown.

Haydo
Posts: 292
Joined: Fri Mar 14, 2003 9:55 am
Location: Eimeo, Qld., Australia
Contact:

Re: Combing with Reactives

Postby Haydo » Tue Sep 16, 2014 8:18 am

Have come back to this over the last few days, thinking whether or not say anything. Congratulations, it's a very thoughtful, well executed piece. Could easily get lost just looking into it. peace, haydo
Life is like a raft, so be like a rat!...Challenging being a captain type rat though, going down with each ship and all!!

Sharol
Posts: 111
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Postby Sharol » Tue Sep 16, 2014 10:21 am

Thanks everyone for the encouraging comments! You stir up my energy!

Sharol

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Combing with Reactives

Postby twin vision glass » Fri Sep 19, 2014 9:54 pm

Glorious, have you worked with the Reactive Ice and Reactive Cloud. I am glad the dense white took the high temperature. Leslie

Sharol
Posts: 111
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Postby Sharol » Sat Sep 20, 2014 10:05 pm

Thank you, Leslie. Yes, I've worked with both in my combings. I particularly like the reactive Cloud, as the reaction seems to be more consistent than the Reactive Ice. Actually, I'm laying a piece up now that will incorporate both along with Lt Aquamarine. Hopefully it will go well and become part of a series.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Combing with Reactives

Postby twin vision glass » Sun Sep 21, 2014 12:39 am

Can hardly waite for the results. Wonderful work . Les

KaCe
Posts: 126
Joined: Sun May 15, 2005 2:25 pm
Location: Old Town, Tacoma, WA
Contact:

Re: Combing with Reactives

Postby KaCe » Sun Sep 21, 2014 3:36 am

What does your combing tool look like? Is it a comb? Or do you use a single tine? I am curious, as I've wanted to try this on some pieces that I didn't like as they are, and thought with some heat and a comb, I could alter it enough to enjoy it. Does it have a long handle? I guess I'm very curious... but grateful for any answers. I do love you design sense and your pallet... very nicely done. =D>

Sharol
Posts: 111
Joined: Sun Mar 05, 2006 2:45 pm
Location: Tennessee

Re: Combing with Reactives

Postby Sharol » Mon Sep 22, 2014 12:19 pm

KaCe -

Here's a photo of my primary raking/combing tool. As you can see it has just one tip. It's about 34.5" from stem to stern and is made from stainless steel rod and tube.

Sharol
Attachments
Rake.JPG

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Combing with Reactives

Postby charlie » Mon Sep 22, 2014 11:23 pm

just remember: unless you have a shutoff switch on the door/lid, part of the comb handle should be wood. this would be pretty dangerous if you didn't have a shutoff switch if you accidentally hit an element.

wood also doesn't conduct heat very well.


Post Reply

Return to “Photos and Stuff”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com