Getting ready to blow out Color Bar in HOT shop
Posted: Mon Apr 16, 2018 11:30 am
by twin vision glass
Hello . I have not posted in awhile and have missed you all so thought I would catch up on what I have been up to. Casting large color bars and then slicing them up to take to the hot shop. Just simply exciting and has allowed me to do things that I could not do before. Working in Bullseye Glass does not stop me from going to the hot shop and Ryan Bavin is truly an inspiration and just knows how to make my ideas and bars into round forms that is a bit more difficult for us all.
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Mon Apr 16, 2018 11:34 am
by twin vision glass
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Mon Apr 16, 2018 1:12 pm
by twin vision glass
![php7epM5dAM.jpg](./download/file.php?id=7564&sid=43e1de33a4d672ef58b7ea30a05ab51d)
- php7epM5dAM.jpg (51.57 KiB) Viewed 31437 times
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Mon Apr 16, 2018 1:13 pm
by twin vision glass
![A piece that is being put back in the kiln to then fuse again and get ready to take to hot shop](./download/file.php?id=7567&sid=43e1de33a4d672ef58b7ea30a05ab51d)
- A piece that is being put back in the kiln to then fuse again and get ready to take to hot shop
- phpATf3rPAM.jpg (42.14 KiB) Viewed 31437 times
![phpKlCEMnAM.jpg](./download/file.php?id=7568&sid=43e1de33a4d672ef58b7ea30a05ab51d)
- phpKlCEMnAM.jpg (45.58 KiB) Viewed 31436 times
![phpSkH4r2AM.jpg](./download/file.php?id=7569&sid=43e1de33a4d672ef58b7ea30a05ab51d)
- phpSkH4r2AM.jpg (50.1 KiB) Viewed 31436 times
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Tue Apr 17, 2018 12:25 am
by Kevin Midgley
impressive work being created.
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Tue Apr 17, 2018 9:25 am
by twin vision glass
Hi Kevin. Hope you are well . I love it back in the hot shop again.
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Tue Apr 17, 2018 9:49 am
by Warren Weiss
Beautiful!! A new dimension.
Warren
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Tue Apr 17, 2018 11:20 am
by twin vision glass
I have really enjoyed getting back into the hot shop and Ryan Bavin just understands so well how the Bullseye Glass Blows out in large chunks and sections and how to maximize the interesting things going on inside. The important part is to remember what will actually be inside when blown out and what is on the outside when all is said and done
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Fri May 11, 2018 2:56 pm
by twin vision glass
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Sat May 12, 2018 8:32 am
by Ed Cantarella
WOW - really gorgeous.
I would really dig manipulating glass like that, after some intense instruction. Too cool.
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Sat May 12, 2018 8:47 am
by twin vision glass
Thank you Ed, I love taking the Bullseye Glass to the hot shop and manipulating it. The large cast glass bars are the best to begin with for me for a more organic look.
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Mon May 21, 2018 10:49 am
by twin vision glass
![phpTpcyNaAM.jpg](./download/file.php?id=7600&sid=43e1de33a4d672ef58b7ea30a05ab51d)
- phpTpcyNaAM.jpg (46.63 KiB) Viewed 31149 times
always fun to go get a nice pic
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Sat Jun 16, 2018 12:22 am
by Sharol
It is so great to see your work posted here again! I’ve missed you! What a wonderful thing for you to once again merge these two glass methodologies. Inspirational. Thank you for posting the pictures of your adventure.
Sharol
Re: Getting ready to blow out Color Bar in HOT shop
Posted: Sat Jun 16, 2018 9:22 am
by twin vision glass
Hi Sharol, It is great to share again with everyone. I tooo have missed posting in Warm Glass.
My twin and I are having fun pulling out the slices on the torch as well. It is just so fun to take this beautiful material and manipulate it hot.