Playing with drop vases

Postby Ed Cantarella » Mon Nov 12, 2018 5:35 pm

All are 10"+
Attachments
bluevase.jpg
multi_vase.jpg
seablue.jpg
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Playing with drop vases

Postby Ed Cantarella » Mon Nov 12, 2018 5:36 pm

Ok, last one. For now. Have 6 others waiting to be beheaded :shock: .
Christmas.jpg
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

Kevin Midgley
Posts: 742
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Playing with drop vases

Postby Kevin Midgley » Fri Nov 16, 2018 12:51 am

Nice work Ed,
The tops don't have to be cut off if you drop the vase onto a nice wide base and fuse them together all at the same time.
Takes making a few duds to get it all perfectly done. :lol:
And all you thought you had to do was perfect the timing and temperature of the drop?
Don't forget the vase will not then go back through the ring so escape planning is required.

Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Playing with drop vases

Postby Ed Cantarella » Sun Nov 18, 2018 10:55 am

Thanks Kevin. Yeah, some we keep the tops on, others cut off. We like breaking, re-arranging and remelting the cut off pieces to make very similar sibling pieces or sets. I've made a few using an escape plan. And a few that couldn't escape - good-bye dear ring. :(
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.


Post Reply

Return to “Photos and Stuff”

Who is online

Users browsing this forum: No registered users and 6 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com