First Combing Try

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
joeat
Posts: 11
Joined: Sat Jan 17, 2004 11:59 pm
Location: Gardner, Kansas

First Combing Try

Post by joeat »

My first attempt at combing, i probably didn't move tool around enough,
but as i said it's my first attempt. Let me know what you think. The help
that i get here makes me want to try new things, and i know that i will
only get good advice.
Thanks
John
http://community.webshots.com/photo/124 ... 0656XtDzuZ
Nutty,Dave
Posts: 9
Joined: Sun Mar 09, 2003 8:06 pm
Location: Sebastopol,CA
Contact:

Post by Nutty,Dave »

i like it !!!

i have not done any combing yet (need some heat protection first) ... what temp did you take it to ???
Peace Through Art !!!
joeat
Posts: 11
Joined: Sat Jan 17, 2004 11:59 pm
Location: Gardner, Kansas

Post by joeat »

I took it to 1700, then i combed, then held at 1700 for 30 min. I was a
little afraid that i would comb too hard and go thru glass into shelf.

John