Postby revjerry » Thu Mar 18, 2004 5:16 pm

I've been playing again and am pretty happy with these pot melts. They measure 18" and are about as big as I can go given my kiln size; guess it's time to buy another one.

Sorry you can't read the description cards. You'll just have to guess at how much I sell these things for.

Image

Anyway, I rely on you folks for critique, but please be gentle.

Jerry

StaceyG
Posts: 40
Joined: Sun Feb 22, 2004 8:17 pm
Location: Baltimore, Maryland

Postby StaceyG » Thu Mar 18, 2004 5:25 pm

These are terrific! Gives us newbies something to aspire to. I've been wanting to try a pot melt, but I have so many other things I want to try to in my little kiln, too!

Stacey

camaro
Posts: 41
Joined: Mon Mar 10, 2003 2:36 pm
Location: Texas

potmelts

Postby camaro » Thu Mar 18, 2004 7:03 pm

WOW !!!!
Those are extrodinary, absolutely beautiful. I wish I knew the the technique, if you'd like to share I'd love to try one my self. I have a large kiln that could handle it.
Excellent job.
camaro

Amy on Salt Spring
Posts: 270
Joined: Sun Mar 09, 2003 5:43 pm
Location: British Columbia, Canada
Contact:

Postby Amy on Salt Spring » Thu Mar 18, 2004 7:05 pm

Any closer upper pictures? I'd love to see the details...
Amy

Debinsandiego
Posts: 41
Joined: Mon May 19, 2003 6:47 pm

Postby Debinsandiego » Thu Mar 18, 2004 7:17 pm

VERY nice work. I like those stands...

I second the motion for close ups. Also, is that a square on the bottom there?? OOHH... I'd like to see that one as well...

:D
Deborah

Rebecca M.
Posts: 126
Joined: Fri Sep 12, 2003 12:15 pm
Location: Myrtle Beach
Contact:

Postby Rebecca M. » Thu Mar 18, 2004 7:31 pm

They look great! Me three want to see close-ups. I am really liking the double rim thing you have going on. 8)

Lisa Allen
Posts: 212
Joined: Sun Mar 09, 2003 3:23 pm
Location: Memphis, TN
Contact:

Postby Lisa Allen » Thu Mar 18, 2004 7:50 pm

I see a girl in the orange one, visible from about the waist up. She is wearing a blue shirt and has red hair and her face is upturned and slightly cocked to her left.........anybody else see her.......or am I having a flashback.

Really cool work!

Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.

revjerry
Posts: 28
Joined: Fri Dec 05, 2003 12:29 pm
Location: Coastal Maine
Contact:

Pot melt detail

Postby revjerry » Thu Mar 18, 2004 8:15 pm

For those kind souls who asked for a detail shot, here it is.
Image

Something in Keith Cummings book got me going on these some time back but I had to be away from them for awhile. Had time to play and it's a good thing. Our season is on the horrizon and I've recieved requests from a couple of galleries. Just now the showroom is pretty full of these things, but that's going to change.

Thanks for the nice comments.

Jerry

revjerry
Posts: 28
Joined: Fri Dec 05, 2003 12:29 pm
Location: Coastal Maine
Contact:

The Stands

Postby revjerry » Thu Mar 18, 2004 8:19 pm

Sorry, I forgot to say that the stands are from Dick Kolpak and can be seen at http://www.ironwoodmetal.com

He makes each one to order. You need to decide which of his you like and tell him the exact size as well as the thickness. Takes about a week but his work is excellent everytime. I have a bunch of his and plan to buy more as I need them.

Jerry

Clifford Ross
Posts: 68
Joined: Sun Mar 09, 2003 10:08 pm
Location: Myrtle Beach, So. Carolina
Contact:

Postby Clifford Ross » Thu Mar 18, 2004 10:29 pm

Just gorgeous!!! The double color outline sharpens attention to the center.
Nice going! :wink: :wink: :wink:

Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Postby Steve Immerman » Thu Mar 18, 2004 11:38 pm

Beautiful!

Steve
Last edited by Steve Immerman on Fri Mar 19, 2004 5:08 pm, edited 1 time in total.

Nickie Jordan
Posts: 39
Joined: Mon Mar 10, 2003 12:16 pm
Location: Palmer, Alaska
Contact:

Postby Nickie Jordan » Thu Mar 18, 2004 11:57 pm

I think your results are amazing ! Thanks for the close-up, absolutely beautiful.

Amy on Salt Spring
Posts: 270
Joined: Sun Mar 09, 2003 5:43 pm
Location: British Columbia, Canada
Contact:

Postby Amy on Salt Spring » Fri Mar 19, 2004 12:04 am

Do you have one of the other one??? I'm greedy, I want to see them both.
Amy

Nancy Juhasz
Posts: 111
Joined: Sun Mar 09, 2003 10:10 pm
Location: Ohio

Postby Nancy Juhasz » Fri Mar 19, 2004 9:16 am

Jerry those are wonderful. I love the orange and blue one. Nanc

Pat Loboda
Posts: 29
Joined: Tue Mar 11, 2003 9:00 pm
Location: Bay City, Michigan
Contact:

Postby Pat Loboda » Fri Mar 19, 2004 10:05 am

I love your pot melts - especially the orange one. I, too, was interested in the stands. Thanks for sharing. The double border definitely gives them distinctiveness & elegance. Glad the galleries are paying attention!

Pat Loboda

Nikki ONeill
Posts: 165
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Postby Nikki ONeill » Fri Mar 19, 2004 10:32 am

Beautiful, Jerry. No muddy interactions, just strong color. Bet that took some testing! They look like planetary images from space, or filtered images of the sun.
Nice work.
Nikki

lindapos
Posts: 4
Joined: Thu Feb 19, 2004 6:02 pm

your work in wonderful

Postby lindapos » Fri Mar 19, 2004 12:17 pm

I am a newbie in glass but your work gives me something to strive for.
Thank you for sharing your work.

Linda Posnick

AZ gram
Posts: 31
Joined: Sat Jan 31, 2004 8:44 pm
Location: Phoenix, AZ
Contact:

WOW!! Just beautiful...

Postby AZ gram » Fri Mar 19, 2004 12:27 pm

I am also new at this. Just tried my first pot melt.

Sure hope you share some of your techniques. :?:

Linda Reed
Posts: 54
Joined: Fri Mar 14, 2003 6:27 pm
Location: Santa Rosa, California, USA
Contact:

Postby Linda Reed » Sat Mar 20, 2004 2:01 am

Those are about as cool as it gets! Very molten, very suggestive of both far off suns and hot places and our own planet core. The colors and the swirls are very evocotive. And of course, nice glass, nicely edged and nicely 'framed'. A total presentation.

Linda

twinkler2
Posts: 45
Joined: Fri Aug 22, 2003 2:37 pm
Location: Happy Valley, PA
Contact:

Postby twinkler2 » Sat Mar 20, 2004 7:59 am

terrific work how big are they?
I love the stands , they really complete the work

Share more pictures?

me kim


Post Reply

Return to “Photos and Stuff”

Who is online

Users browsing this forum: No registered users and 9 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com