Hello,
Can someone please remind me how to calculate the amount of glass I will need for a casting, based on the weight of a clay model?
Thank you!
Calculating amount of glass for a casting by weight of clay?
Moderator: Brad Walker
-
Yardic Glassworks
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Calculating amount of glass for a casting by weight of c
Clays can vary a bit, but when using the low fire clay that I use, it is weight of clay X 1.40 equals glass weight. There are others here who use clay much more than I do, so they may have some additional calculations that they use. Tim
Tim Yardic
Yardic Glassworks
Yardic Glassworks
Re: Calculating amount of glass for a casting by weight of c
Or, you can form the clay into a shape, like say a cube, calculate its volume in cubic centimeters, than take that volume times 2.5 to get the grams of glass that you will need. (2.5 grams/cubic centimeters being the density/specific gravity of Bullseye glass).
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Calculating amount of glass for a casting by weight of c
2.5 is the approximate specific graivity of all soda glass. Lead glass and others are different.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
Re: Calculating amount of glass for a casting by weight of c
or use the water displacement method.. Once you take the clay out of the mould, pour water in... and then use the displacement method...
Re: Calculating amount of glass for a casting by weight of c
Found my notes from an old project. A pretty soft and moist clay. Weight of clay x 1.3 worked perfectly. Thanks everyone.