Hi,
The shelves in my kiln are broken and I cannot buy them in Colombia, where I live. Is it possible to fix them with kaolin or refractory cement?
Is it possible to fix a broken shelf
Moderator: Brad Walker
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Is it possible to fix a broken shelf
You will not be able to repair it so it can be lifted in and out of the kiln in one piece. I suggest instead you level and assemble it (the shelf) in place in the kiln, cover with 1/8" or 1/4" fibreboard or fill cracks with Kaolin then build your glass artwork in the kiln on this assembled shelf.
"The Glassman"