pate de verre-ish

Postby Vonon » Sat Jan 04, 2020 4:03 pm

Is it possible to make a small bowl in a kiln washed mold by pressing glass powder "paste" into the inside surface and tack firing? It seems reasonable as that is a method used for making the "ice bowls" from tempered glass bits. There must be some cosmic force thing I don't recognize that dictates the use of a break away mold. I'm not trying for anything other than a simple little bowl.
Thanks
Vonon

Kevin Midgley
Posts: 722
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: pate de verre-ish

Postby Kevin Midgley » Sat Jan 04, 2020 5:36 pm

watch your temperatures LOL

Look through the files on Warmglass
Like this in the photo section.
http://www.warmglass.com/phpBB3/viewtopic.php?f=3&t=41287&p=351974&hilit=pate+de+verre#p351974

Vonon
Posts: 191
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: pate de verre-ish

Postby Vonon » Mon Jan 06, 2020 2:52 pm

Thanks Kevin. I assume you're cautioning me to keep the temp. low enough to avoid a puddle at the bottom of the pot. I enjoyed revisiting the posts in the archives and was amused to find one of my own in that group.
Vonon

Kevin Midgley
Posts: 722
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: pate de verre-ish

Postby Kevin Midgley » Mon Jan 06, 2020 5:57 pm

Or you need to pack an inner shell holding the carefully placed powder in place.


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 9 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com