So, what are you all casting with now, and what are good suppliers? Some of mine have dried up or downsized since losing Uroboros and Spectrum.

AndyT
Posts: 150
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: casting glass

Postby AndyT » Thu Jan 30, 2020 1:07 pm

Oceanside glasstile is producing cullet in 5lb buckets, 50lbs and 1000lbs sacks. Also Nuggets, Billets, Rocks, and Casting Blocks.
http://artglass.glasstile.com/faq-3

Dick
Posts: 79
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: casting glass

Postby Dick » Thu Jan 30, 2020 1:31 pm

Yeah, reached out to them but have not heard back. i will try them again

Terry Gallentine
Posts: 159
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: casting glass

Postby Terry Gallentine » Fri Jan 31, 2020 1:18 pm

I always used Spectrum Studio Nuggets and still have a back supply. Oceanside has evidently started producing nuggets since they are listed at Delphi. They are however more expensive than the Spectrum nuggets that I purchased a few years ago. When I bought nuggets a few years ago, they cost about a dollar a pound. Delphi has them listed for about $90.00 for fifty pounds or about $1.80 a pound before shipping costs.

Terry Gallentine
Posts: 159
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: casting glass

Postby Terry Gallentine » Fri Jan 31, 2020 1:26 pm

I just checked with Olympic Color (where I got my nuggets a few years ago) and their price for a 50# bag is $62.50. That is not a huge price increase. The trick is in avoiding the freight charges if possible.

Dick
Posts: 79
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: casting glass

Postby Dick » Tue Feb 04, 2020 3:33 pm

So, just FYI Oceanside only carries 96 and no billets rocks or plates. Only nuggets or crushed cullet. Anyone buying billets plates or rocks anywhere besides bullseye? Will be buying BE billets, but looking for options.


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 2 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com