open face casting in reusable clay mold

Post by Paul Tarlow »

Any reason not to make a reusable clay mold for shallow, open face casting (no undercuts)?

- Paul
Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Post by Lauri Levanto »

I have done it several times, to make back reliefs.

The molds tend to be wide, so one must be carefull with drying and firing the mold.

I support the mold on pairs large of kiln brick wedges to
make it level and have enough support area.

In repetive work the separator is a problem.
In full fuse temps it is better to replace the kiln wask
after every fuse. Scaping off from a fine detail mold
is not fun. Instead of kiln wash I use 1-2 ratio
plaster and Al2O3. Maybe 1-4 is enough and parts off easier.

-lauri