I just received from Amazon ($20.) a book entitled "Mould Making for Glass" by Angela Thwaites, copyright 2011, reprint 2012. It's a small (142 pages) softcover.
It contains a wealth of info on the subject supported with many coloured photos.. Seems to be clearly written..
I think this would be a useful addition to warm and hot glass artists reference shelf.
I've paid 3 times as much for bigger books with little useful content.
This one I recommend.
Don
"The Glassman"

Brad Walker
Site Admin
Posts: 1346
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: New Book

Postby Brad Walker » Tue May 28, 2013 12:03 pm

If you can find it, Angela also put together a CD-ROM called "Mixing with the Best" that provided the root material for much of her book. It's basically a survey of glass casters throughout the world and the methods they use in their work. Published in 2002, but long out of print.

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: New Book

Postby Brock » Tue May 28, 2013 12:18 pm

I've got one. I actually responded to the survey, way back when.
Tons of info . . .

Joe Pfeifer
Posts: 24
Joined: Thu May 27, 2010 9:55 pm

Re: New Book

Postby Joe Pfeifer » Wed May 29, 2013 9:15 pm

If someone can find one of the out of print CDROMs, I'd love to buy one.

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: New Book

Postby Morganica » Wed May 29, 2013 9:54 pm

Lots of good info in the CD--the book is pretty much a compilation, better organized and illustrated in the book with some additional material. It's rapidly become one of my favorite glass books, and it's getting rave reviews on Amazon (by me and others):
http://www.amazon.com/Mould-Making-Glass-Handbooks/dp/140811433X/ref=cm_cr-mr-title

The CD, unfortunately, is owned by the university. I contacted them some time ago about re-issuing the CD and they said they had no plans to do so. Possibly the book is the reason.

While we're on the subject of glass books, I'm also really enjoying another one, New Technologies in Glass by Vanessa Cutler. It's not quite as hands-on as Ms. Thwaite's book, and probably doesn't have as many immediate applications, but it's giving me LOTS of ideas. Dr. Cutler lectured on applying new technology to glassmaking at the last BeCON, and this book seems like an extension of her talk. She discusses the use of rapid prototyping systems, computer-controllers and waterjet cutting, bunches more.

http://www.amazon.com/gp/product/1408139545/ref=oh_details_o06_s00_i01?ie=UTF8&psc=1
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Janet McFadyen
Posts: 48
Joined: Mon Aug 28, 2006 4:40 pm
Location: Vancouver Island, BC

Re: New Book

Postby Janet McFadyen » Thu May 30, 2013 3:59 pm

Thanks Don and Cynthia... I ordered the book Janet
facebook artist page @ Janet McFadyen's Glass

seachange
Posts: 223
Joined: Tue Apr 18, 2006 1:19 am

Re: New Book

Postby seachange » Fri May 31, 2013 3:26 am

Thanks Cynthia, I ordered Mould Making and this one http://www.amazon.com/Kiln-Forming-Glas ... pd_sim_b_3

It seemed interesting, couldn't quite decide between this and the one you recommended. Will keep your suggestion in my list for next time.

Best regards, seachange

Nikki ONeill
Posts: 163
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Re: New Book

Postby Nikki ONeill » Mon Jul 22, 2013 7:40 pm

Angela's book is great; a fairly thorough compilation and synthesis of her PhD thesis work. Lots of nuggets there. The CD is a tome to wade through that would be of interest to dedicated casters.
Nikki


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 7 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com