Corderite shelf durability

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
Ron Behrens
Posts: 38
Joined: Wed Jul 24, 2013 8:07 pm

Corderite shelf durability

Post by Ron Behrens »

I have a 21 x 3/4 corderite round shelf with the holes thru it. I was wondering how fast of a rate per hour I could fire it at?
Ron
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Corderite shelf durability

Post by JestersBaubles »

Recommended rate is no more than 200 deg/F per hour for heating and cooling.