Calculating amount of glass for a casting by weight of clay?

Postby Geo » Mon Apr 21, 2014 4:51 pm

Hello,

Can someone please remind me how to calculate the amount of glass I will need for a casting, based on the weight of a clay model?

Thank you!

Yardic Glassworks
Posts: 80
Joined: Sat Mar 06, 2010 9:29 am

Re: Calculating amount of glass for a casting by weight of c

Postby Yardic Glassworks » Mon Apr 21, 2014 5:07 pm

Clays can vary a bit, but when using the low fire clay that I use, it is weight of clay X 1.40 equals glass weight. There are others here who use clay much more than I do, so they may have some additional calculations that they use. Tim
Tim Yardic
Yardic Glassworks

nbobb
Posts: 25
Joined: Mon Aug 16, 2004 1:35 pm
Location: California
Contact:

Re: Calculating amount of glass for a casting by weight of c

Postby nbobb » Thu Apr 24, 2014 5:46 pm

Or, you can form the clay into a shape, like say a cube, calculate its volume in cubic centimeters, than take that volume times 2.5 to get the grams of glass that you will need. (2.5 grams/cubic centimeters being the density/specific gravity of Bullseye glass).
Nancy Bobb
Firewalker Studio
http://www.firewalkerstudio.com

Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Calculating amount of glass for a casting by weight of c

Postby Stephen Richard » Sat Apr 26, 2014 3:58 am

2.5 is the approximate specific graivity of all soda glass. Lead glass and others are different.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/

Soozin
Posts: 11
Joined: Mon Sep 26, 2005 10:40 pm
Location: NEW ZEALAND

Re: Calculating amount of glass for a casting by weight of c

Postby Soozin » Sun May 04, 2014 3:48 am

or use the water displacement method.. Once you take the clay out of the mould, pour water in... and then use the displacement method...

Geo
Posts: 48
Joined: Mon Jul 07, 2003 8:54 am

Re: Calculating amount of glass for a casting by weight of c

Postby Geo » Sun May 04, 2014 4:22 pm

Found my notes from an old project. A pretty soft and moist clay. Weight of clay x 1.3 worked perfectly. Thanks everyone.


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 1 guest

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com