Does anyone know if "Spinel" ramming refractory material would be useful as a component in making your own investment for lost wax casting, or for bead release, or for any other "glass" use?:
Al2O3 89%
SiO2 0.5%
MgO 10%
I have a whole bunch available...
Refractory Materials
Moderator: Brad Walker
-
Joe Pfeifer
- Posts: 24
- Joined: Thu May 27, 2010 9:55 pm
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Refractory Materials
What's it manufactured to be used for?
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Refractory Materials
Ask on craftweb hot glass. They will know.
artist, owner of wanchese art studio, marine finisher
-
Joe Pfeifer
- Posts: 24
- Joined: Thu May 27, 2010 9:55 pm
Re: Refractory Materials
It is a dry ramming material manufactured specifically for use in the installation of pre-formed alumina crucibles and ladles for the steel industry.
http://www.engineeredceramics.com/produ ... erial.html
http://www.engineeredceramics.com/produ ... erial.html
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Refractory Materials
The folks at Craftweb would surely know more about the product than here. If nothing else, Pete has a lot of crucible knowledge.
http://talk.craftweb.com/forumdisplay.php?s=&forumid=4
http://talk.craftweb.com/forumdisplay.php?s=&forumid=4