melted glass on stainless former - WarmGlass.com

melted glass on stainless former

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
jerry keller
Posts: 41
Joined: Sun Mar 30, 2003 11:56 am
Contact:

melted glass on stainless former

Postby jerry keller » Mon Nov 10, 2014 10:56 am

I had a meltdown in the kiln, and have melted glass embedded on a stainless steel former. I tried to get it off by putting in a kiln to 900 degrees, then dropping it into water - a lot of the glass came off, but some remains. I do not want to sandblast it in my booth, as my grit is very fine and I don't want to contaminate it. I was wondering about other techniques to get it off, or also to spray a resist onto it, or kiln wash, and hope that the minor amount of glass still stuck to the surface will not be a problem, as i am just folding vases , not melting glass onto them.

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: melted glass on stainless former

Postby Valerie Adams » Mon Nov 10, 2014 12:29 pm

Do you have diamond hand pads? You may be able to sand it off that way.

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: melted glass on stainless former

Postby Bert Weiss » Mon Nov 10, 2014 12:31 pm

Go to a wholesale restaurant supply and ask for a martini shaker. They cost a small fraction of a floral former from a glass supplier. I bought one from each and they were identical.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

jerry keller
Posts: 41
Joined: Sun Mar 30, 2003 11:56 am
Contact:

Re: melted glass on stainless former

Postby jerry keller » Mon Nov 10, 2014 12:59 pm

IMG_2890.jpg
IMG_2890.jpg (52.49 KiB) Viewed 6853 times
IMG_2890.jpg
IMG_2890.jpg (52.49 KiB) Viewed 6853 times
I also had a ceramic stand that the stainless steel former sat on that got covered with glass. It let the glass slide onto the former, and make the ends of the vase turn a bit. It was 5.5" wide at the base, and was like a gentle slope at the end of the former. Do you have any idea where to get something like this?

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: melted glass on stainless former

Postby rosanna gusler » Mon Nov 10, 2014 6:32 pm

i would dremmel it off. r.
artist, owner of wanchese art studio, marine finisher

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: melted glass on stainless former

Postby charlie » Wed Nov 12, 2014 11:25 pm

[quote="jerry keller"]I had a meltdown in the kiln, and have melted glass embedded on a stainless steel former. I tried to get it off by putting in a kiln to 900 degrees, then dropping it into water - a lot of the glass came off, but some remains. I do not want to sandblast it in my booth, as my grit is very fine and I don't want to contaminate it. I was wondering about other techniques to get it off, or also to spray a resist onto it, or kiln wash, and hope that the minor amount of glass still stuck to the surface will not be a problem, as i am just folding vases , not melting glass onto them.[/quote]

you can sand blast it. it won't contaminate the grit.

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: melted glass on stainless former

Postby Laurie Spray » Thu Dec 04, 2014 2:24 am

Not sure what kind of former.....but if it is one of ours i would just line it with your 1/8" paper and use it. The paper will seperate it from your next work.
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com