Hemp twine, cord as organic material for burnout?

Postby cemoore » Sun Sep 06, 2015 12:27 pm

I'm curious to know if any glass casters on this board have used hemp twine or cord as an organic burnout material. Even if you haven't used this, any thoughts from experienced casters about potential viability?

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Hemp twine, cord as organic material for burnout?

Postby Bert Weiss » Mon Sep 07, 2015 8:08 am

You could destroy the inside of your kiln if you get a big fire inside.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

jim simmons
Posts: 466
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Hemp twine, cord as organic material for burnout?

Postby jim simmons » Mon Sep 07, 2015 1:15 pm

How so ?
Jim

cemoore
Posts: 31
Joined: Mon Aug 11, 2003 10:19 am
Location: Greer, SC

Re: Hemp twine, cord as organic material for burnout?

Postby cemoore » Mon Sep 07, 2015 1:34 pm

Then I could find an alternative means than kiln for burnout.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Hemp twine, cord as organic material for burnout?

Postby Bert Weiss » Mon Sep 07, 2015 11:08 pm

jim simmons wrote:How so ?
Jim
Fire can be very hot, which is hard on elements.

Back in the early 80's my girlfriend was a beginning jeweler. She cast a silver moose, using the lost plastic toy moose method. She burned out the little plastic moose in a kiln. It caught fire and almost ruined the kiln, but it survived. The kiln, of course, was not hers.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions

cemoore
Posts: 31
Joined: Mon Aug 11, 2003 10:19 am
Location: Greer, SC

Re: Hemp twine, cord as organic material for burnout?

Postby cemoore » Tue Sep 08, 2015 9:47 am

Thanks all for your input. I'll be sure not to use the 'lost plastic toy moose' method!

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Hemp twine, cord as organic material for burnout?

Postby Morganica » Thu Oct 22, 2015 1:09 am

Plastic is not the same as hempen twine. For one thing, most plastics aren't organic--many twines are--and if the plastic moose is solid it'd be rather dense and take awhile to burn out (assuming there's enough oxygen around for that). I could see a nice, long, oily petroleum fire, about like burning out petroleum-based wax. Hempen twine, on the other hand, is probably going to burn fast and hot, so it wouldn't be as much of a problem.

For the record, I use organics in mold mixes whenever I have an area of the mold that needs to be weakened, such as a multi-way curve where the glass is going to contract in on itself as it cools. If the mold stayed strong in that area, the glass might crack as it contracted. So I mix old leaves, chopped twine or rope, stale bran cereal, just about anything that won't expand when it gets wet/warm (if it does, it can actually break your mold).

The organics will burn out between 700-1000, leaving a structure that looks strong on the outside but is a bit like swiss cheese in the weakened areas. When the glass starts to contract the plaster can collapse into the hollow spaces instead of having nowhere to go.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Hemp twine, cord as organic material for burnout?

Postby charlie » Thu Oct 22, 2015 9:57 pm

plastic isn't organic? it's a hydrocarbon. organic chemistry is most anything containing of carbon.

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Hemp twine, cord as organic material for burnout?

Postby Morganica » Sun Oct 25, 2015 3:02 am

I stand (very) corrected. Yes, petroleum products are hydrocarbons and therefore contain carbon and are therefore organic. Apparently I have overdone the hippie bit because I have forgotten my organic chemistry and have apparently started using the term "organics" to mean "anything that doesn't contain "petrochemicals." Uhm...ooops.

What I MEANT was... plastics and other petrochemical products I've used tend to leave a sludgey, nasty residue behind in the mold when you heat them to those temps. Hempen twine and similar substances generally burn out completely or at most leave a little light ash behind.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: Google [Bot] and 11 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com