Hi All,

I seem to get soft blisters/bubbles/distentions - not sure what to call them - in my mold face. They arise during steaming and I'm not sure why. In the last mold where this happened, I used two splash coats and a jacket coat, but I'm not necessarily seeing a pattern as I've seen it before with other layer configurations (e.g., one splash coat, one jacket coat) and different investment formulas, usually based on a 50/50 plaster/silica plus maybe some minor amount of EPK to help release and surface smoothness. If I push on one when mold still warm and moist from steam, it will flatten out but then leaves a rough edge or break on the mold face.

Could it be I'm creating a gap of some sort between layers trapping air that I"m not seeing when laying up the coats? If the gap is close enough to the the mold face, that is the 1st layer was fairly thin and fragile, maybe the steam is distorting it?

Thanks

Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Mold Blisters?

Postby Peter Angel » Thu Sep 15, 2016 3:40 am

they might be air bubbles in the mix. Tap the mix bucket down on a hard surface a few times to bring the bubbles to the surface.
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 2 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com