is casting ar 1100c possible

Post by commuted »

I have a vacuum furnace I can set up. I need some electrical work for it. I want to cast glass into a mold. The unit is rated for 1100c. If the glass will slump I'm guessing without air it may conform to a mold. The question is, Is this possible at all at 1100c?
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: is casting ar 1100c possible

Post by Rick Wilton »

at 1000 c you have glass in basically a liquid form, glass blowers have their glass at around that temperature and it's the consistency of honey.

So yes that is plenty hot.

Respectfully though if you are not aware of basic temps I doubt this is something you should undertake.
Rick Wilton