annealing times - WarmGlass.com

annealing times

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
glaskrafter
Posts: 7
Joined: Tue Jan 17, 2012 10:20 am

annealing times

Postby glaskrafter » Wed Mar 01, 2017 4:50 pm

I'm presently doing a fair amount of open face casting. Large salmon that I've scheduled at 2.5 inches. They run 1.5" to 2" thick at the thickest part to 1/4 inch at the thinnest, 24" long X 6" tall. This is very successful. I've noticed that the Bullseye pyramids, although 6" square at the base and 4" tall are scheduled for 2" thick.
I've some larger castings in mind and was curious if anybody has simple way to calculate annealing/cooling time for irregular shaped castings.

Kevin Midgley
Posts: 626
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: annealing times

Postby Kevin Midgley » Wed Mar 01, 2017 5:34 pm

You could just get yourself over to Tofino for a study of a copy of Stone's book and discussion of the actual molds and your firing conditions.
I'd be more than happy to help you out.

glaskrafter
Posts: 7
Joined: Tue Jan 17, 2012 10:20 am

Re: annealing times

Postby glaskrafter » Sat Mar 04, 2017 7:21 pm

Thanks Kevin, go to the wick or down to Ucluelet, Signy's gallery and you can see what I'm doing. Give me a reference to this Stone's book you refer to.

Kevin Midgley
Posts: 626
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: annealing times

Postby Kevin Midgley » Sat Mar 04, 2017 10:34 pm

Well therein likes the problem.
Stone's book does have tons of schedules but you can't just use them without more understanding than being able to copy the timings into a kiln controller.
The bottoms of the pages give you an understanding of what is going on and from that you are able to base your personalized for your molds and kilns schedules.
Thus my suggestion of getting together although you have been pretty successful at what you are doing so if it isn't broken what is there to fix?
I will email you.


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 2 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com