Post by StephenieWooten »

Hello. I recently acquired some molds that were coated in kiln wash. I would like to know if I can remove this wash and apply Boron nitride. And if so what would be the easiest way to remove it? Good ole scrubbing?
Thanks for any suggestions and help.
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Removing kiln wash to apply Boron Nitride

Post by DonMcClennen »

The grid like sandpaper used by drywallers will make short work of removing kilnwash.