The shelves in my kiln are broken and I cannot buy them in Colombia, where I live. Is it possible to fix them with kaolin or refractory cement?

DonMcClennen
Posts: 366
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Is it possible to fix a broken shelf

Postby DonMcClennen » Tue Feb 20, 2018 5:55 pm

You will not be able to repair it so it can be lifted in and out of the kiln in one piece. I suggest instead you level and assemble it (the shelf) in place in the kiln, cover with 1/8" or 1/4" fibreboard or fill cracks with Kaolin then build your glass artwork in the kiln on this assembled shelf.
"The Glassman"


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com