Whiting as texture mold

Postby The Hobbyist » Fri Mar 09, 2018 4:29 pm

Will a nice layer of whiting spread on the shelf with a texture pattern pressed into the surface serve as a mold for kilncarving? Or is it too soft? Can it be stiffened?

Jin "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg

DonMcClennen
Posts: 373
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Whiting as texture mold

Postby DonMcClennen » Fri Mar 09, 2018 5:00 pm

I have mixed whiting with water to a thick cream consistency and applied it to coated kilnshelf with a cake decorating icing sqeezebag to form tree images. Sets to a hard enough image to set 1/4" glass on top. (coat with kilnwash before placing glass on top) You should probably experiment!
"The Glassman"


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 15 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com