Page 1 of 1
Whiting as texture mold
Posted: Fri Mar 09, 2018 4:29 pm
by The Hobbyist
Will a nice layer of whiting spread on the shelf with a texture pattern pressed into the surface serve as a mold for kilncarving? Or is it too soft? Can it be stiffened?
Jin "The Hobbyist"
Re: Whiting as texture mold
Posted: Fri Mar 09, 2018 5:00 pm
by DonMcClennen
I have mixed whiting with water to a thick cream consistency and applied it to coated kilnshelf with a cake decorating icing sqeezebag to form tree images. Sets to a hard enough image to set 1/4" glass on top. (coat with kilnwash before placing glass on top) You should probably experiment!