Postby Peter Zelle » Thu Oct 31, 2019 1:15 pm

Looking for info about R & R glasscast 910.
I am making large (6' x 2') open face molds.
I am casting low relief pieces and am looking for mold material that won't fissure.
I have been using plaster silica mix and fiberglass batting in between layer with some success.
Wondering if R & R might provide better results.

Any info in regards to R & R and avoiding fissures in mold surface, thickness of molds, drying time etc... would be greatly appreciated.

Thanks, Peter

Dick
Posts: 82
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: R & R Glasscast 910

Postby Dick » Sun Nov 10, 2019 7:35 pm

I love r and r. rarely any fissures. I used it for a 38" viking long ship, and for a long cast glass chain. I will try and add a photo or two
IMG_1522279212755[1].jpg
DickDitoreSculpture#4.2008.15x15.jpg

Buttercup
Posts: 552
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: R & R Glasscast 910

Postby Buttercup » Mon Jan 20, 2020 11:15 pm

I just came across these. Very impressive!

Dick
Posts: 82
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: R & R Glasscast 910

Postby Dick » Wed Jan 22, 2020 7:00 pm

Thanks! I hope you were ok through the horrible fires. Being in California I have been through it but you all had it so bad. Thoughts are with you.


Dick

Buttercup
Posts: 552
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: R & R Glasscast 910

Postby Buttercup » Thu Jan 23, 2020 11:25 am

Thank you, Dick. Our area has been OK. Our drought has broken locally but some areas, people and wildlife, have been terribly impacted.

Sadly, today three American air crew died when their water-bomber crashed while fighting the fires near the Snowy Mountains. A tragic loss.


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com