Posted: Sat Jan 04, 2020 4:03 pm
by Vonon
Is it possible to make a small bowl in a kiln washed mold by pressing glass powder "paste" into the inside surface and tack firing? It seems reasonable as that is a method used for making the "ice bowls" from tempered glass bits. There must be some cosmic force thing I don't recognize that dictates the use of a break away mold. I'm not trying for anything other than a simple little bowl.
Thanks

Re: pate de verre-ish

Posted: Sat Jan 04, 2020 5:36 pm
by Kevin Midgley
watch your temperatures LOL

Look through the files on Warmglass
Like this in the photo section.
http://www.warmglass.com/phpBB3/viewtopic.php?f=3&t=41287&p=351974&hilit=pate+de+verre#p351974

Re: pate de verre-ish

Posted: Mon Jan 06, 2020 2:52 pm
by Vonon
Thanks Kevin. I assume you're cautioning me to keep the temp. low enough to avoid a puddle at the bottom of the pot. I enjoyed revisiting the posts in the archives and was amused to find one of my own in that group.

Re: pate de verre-ish

Posted: Mon Jan 06, 2020 5:57 pm
by Kevin Midgley
Or you need to pack an inner shell holding the carefully placed powder in place.