Must I use fusing compatbile glass when doing a casting of a single color and from the same sheet of glass ?

If I'm mixing multiple glass I understand the necessisity to ensure all glasses are compatible. But what about a single color, from same sheet ?

Thanks a ton,
Still a casting newbie.
Russell simms

Brad Walker
Site Admin
Posts: 1345
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Postby Brad Walker » Tue Apr 29, 2003 2:25 pm

Virtually all sheets are compatible with themselves, so if you're using only sheet, you shouldn't have to worry about compatibility.


Post Reply

Return to “Kiln Casting”

Who is online

Users browsing this forum: No registered users and 4 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com