bubbles

Post by ROBFRA »

:? What would it take to get all the bubbles to the surface on a two layer full fuse and smooth back out or not come to the surface at all? When they come to the surface and pop and leave a small crater it looks bad.
Paul Housberg
Posts: 103
Joined: Fri Mar 21, 2003 1:08 pm
Location: Rhode Island
Contact:

Post by Paul Housberg »

Image