fusing riverstones with glass

Post by Paulette »

Can one successfully fuse river stone (small) with glass?

Thanks for your answers...and all the info you give on this board!

Paulette
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: fusing riverstones with glass

Post by Brock »

Paulette wrote:Can one successfully fuse river stone (small) with glass?

Thanks for your answers...and all the info you give on this board!

Paulette
No, you can't. You can combine rocks or stones with slumped glass, but not fused together. You could make a mold of the stones, slump the glass over the mold, then glue the rocks into the depressions. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Barbara Cashman
Posts: 151
Joined: Sun Mar 09, 2003 5:42 pm
Location: Greensboro NC
Contact:

Post by Barbara Cashman »

I remember a long thread about this that should be in the archives. Good luck. - Barbara