Postby jbkramer » Sun Dec 16, 2007 1:40 pm

Hi, I'm new at slumping. Was successful with the first piece, a 6" round bowl. Then I wanted to slump another one, but first had to fire this piece flat. After the second firing, I found this huge bubble at one end. (See picture?) Since I want to slump that piece, should I break open the bubble or will it go away after being slumped? It now has 4 layers of glass. Please advise.

Thanks,
Judy
Attachments
Photo 30.jpg

Deb Lewis
Posts: 9
Joined: Wed Jul 27, 2005 4:54 pm
Location: New Vienna, Ohio
Contact:

Re: A huge bubble

Postby Deb Lewis » Sun Dec 16, 2007 1:49 pm

Welcome to the board, Judy!

First, if you go back to the first topic in the newcomer forum and read it, you'll find we need quite a bit of info to help you.

From the small bubbles that have risen and collapsed, and the large bubble, I'm guessing you are firing too fast and too hot, both beginner errors. Plus, the decor on top probably helped trap the small bubbles. Once we have the firing schedule and other info we will have better answers for you.
My goal in life is to be the kind of person my dog thinks I am.

Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Re: A huge bubble

Postby Barbara Muth » Sun Dec 16, 2007 3:05 pm

looks like you have the dichro between a layer of black and clear. If so, that's why you are trapping so much air.
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS

Deb Lewis
Posts: 9
Joined: Wed Jul 27, 2005 4:54 pm
Location: New Vienna, Ohio
Contact:

Re: A huge bubble

Postby Deb Lewis » Sun Dec 16, 2007 3:16 pm

Duh!!! I should've caught the dichro in the middle, myself!

BTW, Judy, you might want to save the expensive dichro until you have the process down a little better. Glass is expensive enough when you are learning!!
My goal in life is to be the kind of person my dog thinks I am.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 17 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com