Granite Irid
Moderators: Brad Walker, Tony Smith
Granite Irid
What side of the glass is the irid coating on spectrum granite clear?
Thanks,
Robin
Thanks,
Robin
-
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
-
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact:
-
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
I'll have to dig some out to double-check, but the coarse surface is facing up coming through the lehr, so that's the only side that can get sprayed.Mark Kemp wrote:Are you sure about that Tony? All the granite and textured glass I have has the irrid coating on the smooth side. I think at least some of it is Spectrum, but I can't swear to it at this point.Tony Smith wrote:the rough side
tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
The word from Spectrum is that I was mistaken and that you are correct. The regular Spectrum granite, and all their textures for that matter, are iridized on the smooth side. I think my confusion came from the Black System 96 granite being iridized on the rough side and the clear System 96 granite from CBS having the dichroic coating on the rough side. I'm not sure about the clear System 96 granite, but will let you know.Lou_Ohio wrote:I use this glass alot ... irid surface on the smooth side .
Will lose the texture on all glass at fusing tempertures .
Will usually lose the Irid surface at fusing temperture on Spectrum Glass.
Try System 96 or Bullseye to keep Irid surface).
Lou
TOny
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Just an FYI...
And what might confuse the matters worse in the future is that right now most (if not all) of the SYSTEM 96 Irrid glass is actually mfg by Urboros.
However....Spectrum just announced earlier this month that they are now manufacturing their own Hi-Fire Iridecent (starting with a black and clear standard and hopefully adding it to the full S96 color line). Will be interesting to see the pricing on the Spectrum offering as the Urboros....while wonderful glass, is a bit out of line pricing wise with the rest of the System 96 line (at retail cost anyway).
==================
System 96 Hi-Fire Iridescents
Hi-Fire Iridescents with the Spectrum super smooth surface and unsurpassed cutability. We've achieved a satin-like gleam that is as beautiful before firing as it is after. Fire it Irid-side up, Irid-side down - or in between layers. Fire it over and over again. Or, don't fire it at all! The Hi-Fire Irid is a softer look -- very appealing for stained glass work too! We think it's the best Irid ever.
I/100SFS Hi-Fire Iridescent Clear
I/1009SF Hi-Fire Iridescent Black
And what might confuse the matters worse in the future is that right now most (if not all) of the SYSTEM 96 Irrid glass is actually mfg by Urboros.
However....Spectrum just announced earlier this month that they are now manufacturing their own Hi-Fire Iridecent (starting with a black and clear standard and hopefully adding it to the full S96 color line). Will be interesting to see the pricing on the Spectrum offering as the Urboros....while wonderful glass, is a bit out of line pricing wise with the rest of the System 96 line (at retail cost anyway).
==================
System 96 Hi-Fire Iridescents
Hi-Fire Iridescents with the Spectrum super smooth surface and unsurpassed cutability. We've achieved a satin-like gleam that is as beautiful before firing as it is after. Fire it Irid-side up, Irid-side down - or in between layers. Fire it over and over again. Or, don't fire it at all! The Hi-Fire Irid is a softer look -- very appealing for stained glass work too! We think it's the best Irid ever.
I/100SFS Hi-Fire Iridescent Clear
I/1009SF Hi-Fire Iridescent Black
Just an FYI...
And what might confuse the matters worse in the future is that right now most (if not all) of the SYSTEM 96 Irrid glass is actually mfg by Urboros.
However....Spectrum just announced earlier this month that they are now manufacturing their own Hi-Fire Iridecent (starting with a black and clear standard and hopefully adding it to the full S96 color line). Will be interesting to see the pricing on the Spectrum offering as the Urboros....while wonderful glass, is a bit out of line pricing wise with the rest of the System 96 line (at retail cost anyway).
==================
System 96 Hi-Fire Iridescents
Hi-Fire Iridescents with the Spectrum super smooth surface and unsurpassed cutability. We've achieved a satin-like gleam that is as beautiful before firing as it is after. Fire it Irid-side up, Irid-side down - or in between layers. Fire it over and over again. Or, don't fire it at all! The Hi-Fire Irid is a softer look -- very appealing for stained glass work too! We think it's the best Irid ever.
I/100SFS Hi-Fire Iridescent Clear
I/1009SF Hi-Fire Iridescent Black
And what might confuse the matters worse in the future is that right now most (if not all) of the SYSTEM 96 Irrid glass is actually mfg by Urboros.
However....Spectrum just announced earlier this month that they are now manufacturing their own Hi-Fire Iridecent (starting with a black and clear standard and hopefully adding it to the full S96 color line). Will be interesting to see the pricing on the Spectrum offering as the Urboros....while wonderful glass, is a bit out of line pricing wise with the rest of the System 96 line (at retail cost anyway).
==================
System 96 Hi-Fire Iridescents
Hi-Fire Iridescents with the Spectrum super smooth surface and unsurpassed cutability. We've achieved a satin-like gleam that is as beautiful before firing as it is after. Fire it Irid-side up, Irid-side down - or in between layers. Fire it over and over again. Or, don't fire it at all! The Hi-Fire Irid is a softer look -- very appealing for stained glass work too! We think it's the best Irid ever.
I/100SFS Hi-Fire Iridescent Clear
I/1009SF Hi-Fire Iridescent Black
-
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Yeah, actually that was the confusion. Uroboros puts their irid on the rough side, so the System 96 granite, both black and clear, have irid on the rough side (just confirmed by Kat).
Spectrum puts their irid on the smooth side, and the new System 96 glasses should have irid on the smooth side as well.
Tony
Spectrum puts their irid on the smooth side, and the new System 96 glasses should have irid on the smooth side as well.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario