Large Kiln Shelves - Help!!
I have a large L&L kiln that requires a shelf 28" x 42" to fuse large contiguous pieces.  Does anyone know what i can use for a kiln shelf that wil not crack, warp and can hold up to say 80 lbs?
			
			
									
						
										
						- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Large Kiln Shelves - Help!!
My suggestion is Unifrax HD board 1". Thermal Ceramics makes a comparable product, although I think that it doesn't come in 48" and the Unifrax does.J. Allison wrote:I have a large L&L kiln that requires a shelf 28" x 42" to fuse large contiguous pieces. Does anyone know what i can use for a kiln shelf that wil not crack, warp and can hold up to say 80 lbs?
I sugggest using it right on the floor.
I recently heard about a product that works as a rigidizing kiln wash. I won't have the details until next week.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions