dichroic

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
slats
Posts: 110
Joined: Thu Sep 04, 2003 9:19 pm

dichroic

Post by slats »

check out this site. Is anyone familiar with this glass? http://www.graef-dichroic.com/
Sara
Posts: 89
Joined: Wed Mar 12, 2003 9:56 pm
Location: Magdalena, New Mexico, USA

Re: dichroic

Post by Sara »

doctac wrote:check out this site. Is anyone familiar with this glass? http://www.graef-dichroic.com/
Allen has been around since the beyond the very beginnings. At one time he had all his coatings done by GM Vacuum (now Navitar Vacuum Coating Labs) I doubt he's gotten his own chamber but most likely uses either Navitar or CBS, although things could have changed, my info is way old. Many of his patterns are/were exclusive to him when he was having them coated.

Good glass, good patterns.

Sara
Post Reply