Postby Richard Sinning » Tue Feb 17, 2004 3:43 pm

When fusing float, as I understand it the two tin sides must be facing each other. If you fuse 3 pieces of float does the 3rd piece face inward? TIA
Richard

Glenda Kronke
Posts: 64
Joined: Tue Mar 11, 2003 11:44 am
Location: Austin, TX
Contact:

Postby Glenda Kronke » Tue Feb 17, 2004 3:48 pm

Richard,

I think the main thing you are trying to avoid is devit. Tin side devits much easier than the air side. So, rule of thumb is 'tin side down' , espicially on the top piece of glass-IMO.

Hope this helps.

g-

Bobcat
Posts: 7
Joined: Wed Jan 28, 2004 3:42 pm
Location: Bozeman, MT

Postby Bobcat » Tue Feb 17, 2004 4:08 pm

Will devit sprays or borax help the piece if tin side is up?

I'm new to this too and am borrowing kiln time this weekend for some float projects this weekend.

So any tips regarding the tin side of float glass would be greatly appreciated.

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Postby Bert Weiss » Wed Feb 18, 2004 12:51 am

I don't find the tin side more prone to devit, exactly. The tin side does protect the bottom surface when placed against the shelf.

The tin side can effect enamels making them turn brown, so if you are enameling keep the tin side away from the enamels.

I find fewer devit problems using heavier glasses 10mm and up are less prone than 1/4" and thinner.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 49 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron